I have had a problem with matt emulsion (dulux). after application with a pad, after a few mins, tiny bubbles form in patches. This was the second coat applied 1 hr after the first. They seem to be hollow. These only appeared on one area of one wall. Could accidental spraying of hair spray/ deodrant onto wall cause this or is it another issueie not waiting long enough before applying second coat?
 
Sponsored Links
Do the 'bubbles' resemble little rings.....the sort of things that appear when water goes onto a greasy surface?
 
not really rings -just tiny blisters ranging from 1-3mm dia. if you wipe over them quite hard with a damp cloth they will dissipate back into the paint.
 
Sponsored Links
Ive seen that happen before over filler.

Or they could be down to the coating underneath lifting so some reason..the water in the emulsion you apply is soaking through the coating underneath and causing that to lift from whatever is underneath that.

They normally dry back after a few hours.....if you have to push them down again give the wall a coat of oil based undercoat first then apply the emulsion.
 

DIYnot Local

Staff member

If you need to find a tradesperson to get your job done, please try our local search below, or if you are doing it yourself you can find suppliers local to you.

Select the supplier or trade you require, enter your location to begin your search.


Are you a trade or supplier? You can create your listing free at DIYnot Local

 
Back
Top