Hi all
Had a go at GRP-ing my shed roof and got caught out by weather on about 1 square metre. This section has hardened but has pin holes in the top coat.
What is the correct way to rectify this? Sand the affected area, add resin then re-top coat?
Or is more matting required once sanded?
Any help much appreciated.